Avimetal / AM0308

Hastelloy X Superalloy

Nickel powdersMetal laser powder bed fusion

A nickel-based superalloy powder for temperature- and corrosion-focused metal-AM component development.

Material systemNickel-based superalloy
ProcessMetal laser powder bed fusion
Supply formatPrinting powder; bag, bottle or drum size confirmed with quotation
Commercial termsQuotation on specification and quantity
Ask about samples

No online checkout. Confirm grade, availability, MOQ and terms before ordering.

MATERIAL POSITIONING

Features & applications

Typical applications

High-temperature component developmentHeat exchangersCorrosion-focused components

MATERIAL DETAIL

Powder microscopy

These source micrographs describe particle appearance. Use the grade specification and batch report to check particle distribution; a photograph does not establish a complete PSD.

Manufacturer SEM photograph of Hastelloy X Superalloy powder, from its grade TDS (page 1).
Manufacturer SEM photograph of Hastelloy X Superalloy powder, from its grade TDS (page 1). Source reference ↗

EXACT-GRADE INFORMATION

Technical specifications

ParameterSource-reported value
Source grade / productHastelloy X SuperalloyManufacturer / source information
Material systemNickel-based superalloyManufacturer / source information
Printing processMetal laser powder bed fusionProcessing guidance
Particle-size D10≥15 µmFeedstock property
Particle-size D5030-40 µmFeedstock property
Particle-size D90≤60 µmFeedstock property
Sphericity≥0.9Feedstock property
Loose density≥4.4 g/cm³Feedstock property
Flowability≤18 s/50 gFeedstock property
Tap density≥5.0 g/cm³Feedstock property

See the cited technical document for test conditions, print orientation and post-processing. Include any required batch reports in your inquiry.

CHECK THE COMPLETE PROCESS

Printer & machine requirements

  • Confirm the machine laser system, atmosphere and grade-specific build parameters.
  • Specify PSD, oxygen/interstitial limits and flow requirements with the inquiry.
  • Qualify the build and heat-treatment route for the intended component.
Check this grade against your machine

CONTINUE YOUR SELECTION

Compare related materials.

All metal powder

FIND YOUR MATERIAL

Search by grade, material, original brand or printing process.

MATERIALS · WHOLESALE · OEM

Request a quotation

Tell us the material, machine and quantity. Choose email or WhatsApp for the next step.

Your request is submitted to our sales team. No payment is collected.